Copper · Brass · isotropic

CuZn37 brass (CW508L)

EN 1652 · 20 °C

CuZn37 brass (CW508L) is a brass to EN 1652. E = 105 GPa, ν = 0.34 and α = 20.2 × 10⁻⁶/K (typical values).

Record
cuzn37
Library
v1.1.0
Properties
8
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 105GPa typical[1]
ν · Poisson's ratio 0.34– typical[1]
ρ · Density 8440kg/m³ typical[1]
α · Coefficient of thermal expansion 20.210⁻⁶/K typical[1]
λ · Thermal conductivity 120W/(m·K) typical[1]
c_p · Specific heat capacity 377J/(kg·K) typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus 105 GPa typical [1]
ν Poisson's ratio 0.34 – typical [1]
K Bulk modulus K = E / 3(1 − 2ν) 109.4 GPa derived —
λ_L Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) 83.26 GPa derived —
c₀ Bar wave speed c₀ = √(E/ρ) 3527 m/s derived —

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density 8440 kg/m³ typical [1]
α Coefficient of thermal expansion ⓘ 0–300 °C 20.2 10⁻⁶/K typical [1]
λ Thermal conductivity 120 W/(m·K) typical [1]
c_p Specific heat capacity 377 J/(kg·K) typical [1]
σ_e Electrical conductivity 15 MS/m typical [1]
IACS Conductivity relative to annealed copper 26 % typical [1]
a Thermal diffusivity a = λ / (ρ·c_p) 37.71 mm²/s derived —

Notes

  • Strength depends on the temper; see the producer's table.

Sources

every value names one
  1. Wieland M37 (CuZn37, CW508L) datasheetCopies checked: 1

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). CuZn37 brass (CW508L) — material properties, EN 1652. Library v1.1.0, record cuzn37. https://www.badgermecx.com/materials/cuzn37/ (accessed 2026-11-26).

@misc{badgermecx_cuzn37,
  title  = {CuZn37 brass (CW508L) -- material properties, EN 1652},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record cuzn37},
  url    = {https://www.badgermecx.com/materials/cuzn37/}
}

Export and related

SI units, every value with basis and source