Nickel · Nickel alloy · isotropic

Alloy 625 (UNS N06625)

Special Metals INCONEL 625 · annealed, about 21 °C

Alloy 625 (UNS N06625) is a nickel alloy to Special Metals INCONEL 625. Its typical yield strength is 414 MPa. E = 207.5 GPa, ν = 0.278 (typical values).

Record
ni-625
Library
v1.1.0
Properties
9
Sources
1
Build check
passed ✓
Viewing as
guest
+ Compare Cite Download · PRO
E · Young's modulus 207.5GPa typical[1]
ν · Poisson's ratio 0.278– typical[1]
f_y · Yield strength (R_eH / R_p0.2) 414MPa typical[1]
f_u · Tensile strength (R_m) 827MPa typical[1]
ρ · Density 8440kg/m³ typical[1]
λ · Thermal conductivity 9.8W/(m·K) typical[1]
c_p · Specific heat capacity 410J/(kg·K) typical[1]

Elastic constants

isotropic
SymbolPropertyValueUnitBasisRef.
E Young's modulus 207.5 GPa typical [1]
G Shear modulus 81.4 GPa typical [1]
ν Poisson's ratio 0.278 – typical [1]
K Bulk modulus K = E / 3(1 − 2ν) 155.8 GPa derived —
λ_L Lamé constant λ_L = Eν / (1 + ν)(1 − 2ν) 101.7 GPa derived —
c₀ Bar wave speed c₀ = √(E/ρ) 4958 m/s derived —

Physical, thermal and electrical

at 20 °C
SymbolPropertyValueUnitBasisRef.
ρ Density 8440 kg/m³ typical [1]
λ Thermal conductivity 9.8 W/(m·K) typical [1]
c_p Specific heat capacity 410 J/(kg·K) typical [1]
ρ_e Electrical resistivity ⓘ 129 µΩ·cm 1.29 µΩ·m typical [1]
a Thermal diffusivity a = λ / (ρ·c_p) 2.832 mm²/s derived —

Strength

a band applies up to and including its upper limit
SymbolPropertyValueUnitBasisRef.
f_y Yield strength (R_eH / R_p0.2) ⓘ annealed rod, bar and plate 414 (414 – 655) MPa typical [1]
f_u Tensile strength (R_m) ⓘ annealed rod, bar and plate 827 (827 – 1034) MPa typical [1]

Sources

every value names one
  1. Special Metals, INCONEL alloy 625 technical bulletinCopies checked: 1

min product standard minimum char characteristic design code value for design typical datasheet or textbook derived worked out here, formula shown

Cite this page

for reports and papers

BadgerMecX Materials (2026). Alloy 625 (UNS N06625) — material properties, Special Metals INCONEL 625. Library v1.1.0, record ni-625. https://www.badgermecx.com/materials/ni-625/ (accessed 2026-11-26).

@misc{badgermecx_ni625,
  title  = {Alloy 625 (UNS N06625) -- material properties, Special Metals INCONEL 625},
  author = {{BadgerMecX Materials}},
  year   = {2026},
  note   = {Library v1.1.0, record ni-625},
  url    = {https://www.badgermecx.com/materials/ni-625/}
}

Export and related